  • Omni Turn Spindle Rebuild

    Omni Turn Spindle Repair

    Omni Turn Spindle Repair

    Lathe

    4,000 rpm

    We received this from a company that produces precision parts for the medical, automotive and electronics industries. The spindle had 70 microns of run out in the taper. The customer needed better run out in order to provide their customers with quality parts.

    It was determined that the taper would need grind, chrome plate and finish grind. The shaft was sent into our grinding department and they were able to bring the taper back to 2 microns of run out. After assembly and inspection the spindle was sent to the customer. They were very satisfied with the run out on the spindle and its performance in the machine.



    Fischer MFN 1045
    Fischer MFN 1045

    Fischer MFN 1045

    45,000 rpm
    ID grinding spindle
    This spindle was crashed causing damage to the front bearing journal and the ID tooling pilot. It was necessary to grind plate grind the front journal and the pilot. We then assembled the spindle and test ran it at 45,000 rpm. After final balance and passage of our stringent final QC standards the spindle was shipped back to our customer.


    Okuma Howa 550H
    Okuma Howa 550H

    Okuma Howa 550H

    6000 rpm
    Stator driven
    Spindle was crashed, shaft nose was cracked, rotor came loose and rubbed out on rear housing.  Rear housing was egged shaped.  The taper had 20+ microns of runout.
    Northland Tool & Electronics replaced the bearings, ground/plate/ground the rear housing and 50 taper.  Kiss ground the front journal and shoulders.  Welded and machined the cracks in shaft nose.


    NSK LZ 24B82

    NSK LZ 24B82

    Rear bearing failure. Rear bearing journal was undersized. Drawbar nut was seized to the shaft and needed to be machined off. Front bearings were contaminated. Taper was bellmouthed, tool only contacts in the rear of the taper.
    Work done:
    Grind plate grind rear shaft journal. Kiss grind taper. Manufacture new drawbar nut. Replace belleville washers on drawbar.Clean, inspect overall dimensions. Replace bearings, adjust preload, balance, assemble and break in. Final quality control inspection.


    Pope P-924-GA
    Pope P-924-GA

    Pope P-924-GA

    3600 rpm
    Grinding spindle
    This type of spindle can be used to manufacture broaches, drill bits, tooling and also has many other applications. We have been repairing this type of spindle for more than 20 years.


    Kitamura H-400
    Kitamura H-400

    Kitamura H-400

    10,000 rpm
    This spindle needed a grind plate grind to the taper and the front bearing housing. After completion of the grinding the spindle was assembled, test run and balanced.